Our R & D team

All of them are engineers with at least 10 years of experience in plastic bottle equipment

Our Advantages

Provide all equipment for PET plastic bottle equipment, one-stop shopping

Our Services

The repurchase rate exceeds 50%, customers give consistent praise, and the shelf life is at least 24 months.

Why Choose Us?

As a 20-year-old Chinese factory specializing in PET plastic bottle packaging equipment, we bring extensive experience and quality to every project. Our main offerings—blow molding machines, blow molds, and complete filling line solutions—provide clients with a comprehensive, reliable one-stop solution from design to installation.

Our factory is equipped with advanced precision machinery, and we have a team of over 20 highly experienced R&D engineers, each with more than 10 years in the industry. This expertise enables us to deliver efficient, durable, and high-performance equipment that meets diverse client needs across industries.

In addition to our high standards in production, we pride ourselves on our skilled installation team and responsive after-sales service, ensuring that clients receive continuous support and seamless operation from day one.

What sets us apart is our commitment to customer satisfaction through customized, client-driven solutions. We understand the critical importance of production efficiency and consistent quality, and our dedicated team is here to provide trusted solutions that empower your business. Choose us as your partner for quality, reliability, and value in PET packaging solutions.

 

main products

bottle design free

Experience excellence with us – we offer free bottle design and prototyping. Let us shape your ideas into reality!

water bottle mold
1-12 cavities
7025 Aluminum
3 million times
after-sale warranty
Oil bottle mold
1-4 cavities
7025 Aluminum
High-Quality
after-sale warranty

20 years of physical factory

Jindong Machinery has a self-built factory building of 8,000m³ and a 20-year history.

Our Strength

Manufacturing Capabilities

We sell 120 sets of automatic bottle blowing machines every year, and our customers are in 20 countries.

Quality and Service

We always focus on product quality and after-sales service, and can provide a variety of technical support such as online and on-site.

Four-step ordering

Requirement Communication

 Communicate via phone or online to understand your production needs, including bottle design, output requirements, and budget, ensuring the best automatic blow molding machine solution is recommended.

Solution Confirmation

Based on your requirements, provide a detailed plan covering equipment specifications, mold design, and process workflows to ensure the product meets market and filling standards.

Contract Signing

Description: Once both parties agree, sign the purchase contract. After receiving your deposit, we will arrange production and equipment testing to ensure quality and timely delivery.

Equipment Delivery

Description: Upon production completion, we arrange transportation and provide on-site installation, commissioning, and operational training to ensure smooth production startup.

Online free courses with Steve Robinson

Earn Digital Marketing Skills To Boost Up Your Business.

Course 1

How to make your social media content go viral

Lorem ipsum dolor sit amet, consectetur adipiscing elit. aulla sit amet magna sodales, interdum tortor etlert of dictum mauris loean ultricies lectus quis gravida urna interdum quam bibend.

How to make your social media content go viral

5 lessons - 4:11 hours
View Course

Course 2

How to build a successful email newsletter

Lorem ipsum dolor sit amet, consectetur adipiscing elit. aulla sit amet magna sodales, interdum tortor etlert of dictum mauris loean ultricies lectus quis gravida urna interdum quam bibend.

How to build a successful email newsletter

5 lessons - 4:11 hours
View Course

Course 3

How to use online reviews to boost your business

Lorem ipsum dolor sit amet, consectetur adipiscing elit. aulla sit amet magna sodales, interdum tortor etlert of dictum mauris loean ultricies lectus quis gravida urna interdum quam bibend.

How to use online reviews to boost your business

5 lessons - 4:11 hours
View Course

Course 4

Best Practices For Linkedin Features Used For Social Recruiting

Lorem ipsum dolor sit amet, consectetur adipiscing elit. aulla sit amet magna sodales, interdum tortor etlert of dictum mauris loean ultricies lectus quis gravida urna interdum quam bibend.

Best Practices For Linkedin Features Used For Social Recruiting

5 lessons - 4:11 hours
View Course

Tip 1

Tips for ensuring efficient operation of equipment

Regular maintenance of PET blow molding machines
In order to extend the service life of PET blow molding machines and improve production efficiency, regular maintenance is essential. It is recommended to clean the heating lamps monthly, check the gas system for leaks, and add lubricating oil to the moving parts. Perform a detailed inspection of key components such as the electrical system and cylinders every quarter to ensure that the equipment is normal. Proper maintenance can avoid downtime and improve production efficiency.

Tip 1

Mold maintenance, reduce unnecessary losses

Cleaning and inspection of preform molds
The precision of preform molds directly affects product quality, so it is necessary to clean the inner and outer surfaces of the mold regularly to remove residues or dust. Check whether the mold is worn or deformed to ensure that the mold is tightly closed. It is recommended to use professional tools to polish the mold every six months to extend the service life of the mold and ensure stable molding quality.

Tip 1

Improve product quality, start from details

Subheadline: Maintenance of cooling system of blow mold
The cooling system of blow mold is a key component to ensure the quality of finished products. Clean the scale or impurities in the cooling water channel regularly to ensure cooling efficiency. Check whether the mold seal is aging to avoid cooling water leakage affecting production. Good cooling system maintenance helps to improve the transparency and strength of the bottle.

Tip 1

Clean Equipment Regularly

Remove dust and debris daily to ensure smooth operation and prevent system blockages.

Hey!

I am Vivian,

I would like to remind you that when using PET bottle blowing equipment, daily maintenance is the key to keeping the equipment running efficiently. Here are some simple but practical daily maintenance suggestions for you, hoping to help you manage the equipment better

Hey!

I am Vivian,

I would like to remind you that when using PET bottle blowing equipment, daily maintenance is the key to keeping the equipment running efficiently. Here are some simple but practical daily maintenance suggestions for you, hoping to help you manage the equipment better

Clean Equipment Regularly

Remove dust and debris daily to ensure smooth operation and prevent system blockages.

Inspect Air Systems

Check for leaks and maintain stable pressure to enhance machine efficiency.

Lubricate Moving Parts

Apply lubricant to key components to reduce friction and extend equipment life.

Some Feedbacks

What people are saying

main products

Provide one-stop customized solutions for PET plastic packaging from injection blow molding to filling.

main products

Provide one-stop customized solutions for PET plastic packaging from injection blow molding to filling.

Our Case

32-cavity preform case

500ML water bottle 2400pcs/h Case

Violent Bear 2000pcs/h Case

Large mouth jar 2000pcs/h case

15L bottled water 300pcs/h case

15L bottled water 1200pcs/h case

500ML mineral water 9000pcs/h

700ML Mouthwash 1000pcs/hour

We have successfully provided thousands of complete solutions to customers around the world, covering the unique needs of various industries. Whether it is a start-up factory or a large-scale production enterprise, we can customize efficient and stable production lines to help customers seize market opportunities.

Output: 1000pcs/h, Maximum capacity: 3L

Output: 500pcs/h, Maximum capacity: 5L

Output: 300pcs/h, Maximum capacity: 20L

NO. Name Parameters Name Parameters
1 Number of cavities 2 cavities Maximum capacity 5L
2 Output 800PCS/H Maximum bottle mouth diameter 120MM
3 Power 15kw Total machine weight 1.5T

This bottle blowing machine has a higher output than the single-chamber 5L bottle blowing machine. It is suitable for factories that require slightly higher output but do not want to buy automatic machines. It is affordable and easy to operate.

NO. Name Parameters Name Parameters
1 Number of cavities 4 cavities Maximum capacity 1L
2 Output 1800PCS/H Maximum bottle mouth diameter 30MM
3 Power 15kw Total machine weight 1.5T

Compared with other semi-automatic blow molding machines, this blow molding machine has the advantage of high output and is cheaper than automatic machines. It is suitable for start-up small-scale factories.

NO. Name Parameters Name Parameters
1 Number of cavities 1 cavities Maximum capacity 20L
2 Output 300PCS/H Maximum bottle mouth diameter 120MM
3 Power 18kw Total machine weight 1.8T

This 20L bottle blowing machine is suitable for producing five-gallon bottled water and disposable bottled water. Compared with the large investment of automatic machines, this one has the advantages of short installation time, easy operation and high output.

NO. Name Parameters Name Parameters
1 Number of cavities 1 cavities Maximum capacity 20L
2 Output 300PCS/H Maximum bottle mouth diameter 130MM
3 Power 40kw Total machine weight 1.5T

This bottle blowing machine is suitable for the production of 5-20L bottles and has a wide range of applications. Disposable bottled water is the current trend. This semi-automatic bottle blowing machine occupies little space, has a favorable price, is easy to operate, and is very popular.

NO. Name Parameters Name Parameters
1 Number of cavities 32 cavities Preform weight 25g
2 Output 4600PCS/H Preform diameter 3025
3 One cycle 25S Total machine weight 1.5T

Our preform molds do not turn white or draw wire, have stable hot runners, short cooling cycles, smooth demoulding, and high overall mold precision.

NO. Name Parameters Name Parameters
1 Number of cavities 2 cavities Maximum capacity 2L
2 Output 2000PCS/H Maximum bottle mouth diameter 38MM
3 Power 32kw Total machine weight 2.5T

This bottle blowing machine is suitable for bottles such as water and beverages. It has a wide range of applications and is easy to operate, making it suitable for small and medium-sized factories.

NO. Name Parameters Name Parameters
1 Number of cavities 2 cavities Maximum capacity 2L
2 Output 1500PCS/H Maximum bottle mouth diameter 120MM
3 Power 42kw Total machine weight 3.5T

This bottle blowing machine is suitable for wide-mouth jars, has high output, is suitable for connecting to the entire injection molding line, and is suitable for automated factories.

NO. Name Parameters Name Parameters
1 Number of cavities 4 cavities Maximum capacity 0.8L
2 Output 6000PCS/H Maximum bottle mouth diameter 38MM
3 Power 48kw Total machine weight 4.5T

This bottle blowing machine is suitable for water bottles, beverage bottles, etc., and is suitable for connecting to the entire production line of filling machines. It is suitable for small and medium-sized automated factories.

NO. Name Parameters Name Parameters
1 Number of cavities 4 cavities Maximum capacity 2L
2 Output 5000PCS/H Maximum bottle mouth diameter 38MM
3 Power 48kw Total machine weight 5T

This bottle blowing machine is suitable for water bottles and beverage bottles within 2L, etc. It has a high degree of automation and stable machine, and is suitable for factories that want to improve efficiency.

NO. Name Parameters Name Parameters
1 Number of cavities 6 cavities Maximum capacity 0.8L
2 Output 9000PCS/H Maximum bottle mouth diameter 30MM
3 Power 64kw Total machine weight 6T

This bottle blowing machine is suitable for small-capacity PET bottles and can be connected to the filling machine for production. The equipment has a high degree of automation and more than 90% of its components are internationally renowned brands.

NO. Name Parameters Name Parameters
1 Number of cavities 8 cavities Maximum capacity 0.8L
2 Output 12000PCS/H Maximum bottle mouth diameter 30MM
3 Power 86kw Total machine weight 8T

The 8-cavity fully automatic bottle blowing machine is suitable for bottled water bottles below 800ml, and is connected to a 12000 filling machine line, which is suitable for water beverage factories that require high efficiency and automation.

NO. Name Parameters Name Parameters
1 Number of cavities 1 Cavities Maximum capacity 0-5L
2 Material 6061T Aluminum Surface treatment Hard anodized
3 Suitable for models Rotary Blow Molding Machine Bottle Type Water bottles, soda, etc.
NO. Name Parameters Name Parameters
1 Number of cavities 10 Cavities Maximum capacity 0-0.8L
2 Material 7075 Aluminum Surface treatment Polishing
3 Suitable for models Linear automatic bottle blowing machine Bottle Type Water bottles, soda, etc.
NO. Name Parameters Name Parameters
1 Number of cavities 2 Cavities Maximum capacity 0-2L
2 Material S136 Stainless steel Surface treatment Polishing
3 Suitable for models Linear automatic bottle blowing machine Bottle Type Wide-mouth jars, daily chemical bottles, etc.
NO. Name Parameters Name Parameters
1 Number of cavities 2 Cavities Maximum capacity 0-1L
2 Material S136 Stainless steel Surface treatment Polishing
3 Suitable for models Linear automatic bottle blowing machine Bottle Type Wide-mouth jars, daily chemical bottles, etc.
NO. Name Parameters Name Parameters
1 Number of cavities 6 Cavities Maximum capacity 0-0.8L
2 Material 7075 Aluminum Surface treatment Polishing
3 Suitable for models Linear automatic bottle blowing machine Bottle Type Water bottles, beverage bottles, daily chemical bottles, etc.
NO. Name Parameters Name Parameters
1 Number of cavities 1 Cavities Maximum capacity 5-20L
2 Material 7075 Aluminum Surface treatment Polishing
3 Suitable for models Linear automatic bottle blowing machine Bottle Type Bottled water, oil bottles, etc.
NO. Name Parameters Name Parameters
1 Number of cavities 2 Cavities Maximum capacity 0-10L
2 Material 7075 Aluminum Surface treatment Polishing
3 Suitable for models Semi-automatic bottle blowing machine Bottle Type Water bottles, beverage bottles, etc.
NO. Name Parameters Name Parameters
1 Number of cavities 2 Cavities Maximum capacity 0-15L
2 Material 7075 Aluminum Surface treatment Polishing
3 Suitable for models Linear automatic bottle blowing machine Bottle Type Oil bottles, barreled water bottles, etc.
NO. Name Parameters Name Parameters
1 Number of cavities 2 Cavities Maximum capacity 0-30L
2 Material 7075 Aluminum Surface treatment Polishing
3 Suitable for models Semi-automatic bottle blowing machine Bottle Type Oil bottles, barreled water bottles, etc.
Semi-automatic bottle blowing machine mold
1 -4 cavities
Material: Aluminum or stainless steel
Caliber:International standard
Oil bottle mold
1 -2 cavities
Material: Aluminum or stainless steel
Caliber:International standard
Bottled water mold
1 cavities
Material: 7075 aviation aluminum
Caliber:International standard
Daily chemical bottle mould
1 -8 cavities
Material: 7075 aviation aluminum
Caliber:International standard
6-cavity blow molding mold
6 cavities
Material: 7075 aviation aluminum
Caliber:International standard
Disposable bottled water mold
1 -2 cavities
Material: 7075 aviation aluminum
Caliber:International standard

Our Classes

Lorem ipsum dolor sit amet, consectet adipiscing elit,sed do eiusm por inciunt ut labore et dolore magna aliqua. Ut enim ad minim veniam, quis nostrud exercitation ullamco laboris nisi ut aliquip ex ea sint occaecat cupidatat non proident, sunt in culpa qui officia mollit natoque consequat massa quis enim.


Nam quam nunc, blandit vel, ridiculus mus. Donec quam Lorem ipsum dolor sit amet, consectet adipiscing elit,sed do eiusm por incididunt ut labore et dolore magna aliqua.

Reason
1. Insufficient temperature of hot runner
2. Insufficient material temperature
Elimination method:
1. Strengthen heat insulation measures 2 . Increase the temperature of the nozzle here 3 . Properly increase the material temperature 4. Speed up the injection speed5. Reduce the holding pressure6. slow down cooling water flow

Reason:
1. Insufficient drying of raw materials
2. Insufficient plasticization of raw materials
3. pp> preform wall thickness is too large or insufficient cooling
4. mixed with other plastics
5. Material temperature is too low
Elimination method:
1 Guaranteed to dry for more than four hours 2. Raise the material temperature 3. Increase the screw speed 4. Check whether the temperature of the drying material is too low or the injection volume does not match. It is necessary to ensure that the raw material is dried at 165 degrees until the moisture content is less than 0.02%. 5. Enhanced cooling, thinner wall thickness

Reason:
1. Holding pressure too high
2. Bottom film gate hole eccentric
Elimination method:
1. reduce stress
2. Correction mold

Reason:
Insufficient drying
Elimination method:
1. Strengthen drying 2. Increase material temperature 3. Reduce screw speed

Reason:
1. Material temperature is too high
2. injection rate is too short
3. Dwell too short
4. Injection time is too short
5. Insufficient cooling
Elimination method:
1. Lower material temperature
2. Reduce the injection rate
3. increase pressure
4. increase injection time
5. increase water pressure

Reason:
1. Poor insulation
2. Insufficient cooling
3. pressure in heat flow
4. Bad screw check
5. Holding pressure too low
Elimination method:
1. Guaranteed heat insulation at the gate
2. increase cooling
3. Reinforce the inverted cable
4. Clean the screw nozzle
5. increase pressure

Reason:
1. Gate hole eccentric
2. uneven cooling
Elimination method:
1. Correct mold 2. Reduce the holding pressure
3. Increase injection speed 4. extended cooling
5. Clean up waterways 6. Increase cooling water pressure

Reason:
1. Poor mold manufacturing
2. Gate hole deviation
3. Injection pressure too high
4. core shift
Elimination method:
1. Correction mold
2. Raise material temperature
3. turn down the pressure
4. Mold with high strength, high precision and adjustable core structure

reason:

1. The heating temperature is too high. 2. The heating time is too long. 3. Compressed air contains moisture. 4. The embryonic tube itself is opaque. 5. The embryo tube design is inappropriate. 6. The inflation rate is too small

Elimination method:

1. Lower the temperature 2. Shorten the heating time 3. Use a dryer to remove moisture 4. Improve the quality of the embryo tube, select materials, and increase the dryness of the raw materials 5. Improve the size design of the embryo tube 6. Reduce the diameter of the preform.

reason:

1. The heating temperature is too low. 2. The embryonic tube wall thickness is uneven. 3. The thickness of the embryo tube is too thick and the heating penetration is insufficient.

Elimination method:

1. Increase the temperature or slow down the rotation speed 2. Improve the quality of the embryo tube 3. Reduce the thickness of the embryo tube, or try to add a heating device cover to increase the temperature distribution surface of the preform.

reason:

1. The blowing time is too early 2. The stretching rod has not been lowered to the bottom 3. The stretching rod deviates from the center line of the bottle axis 4. The wall thickness of the embryo tube is uneven or the injection density is uneven 5. Uneven heating

Elimination method:

1. Delay the blowing time or increase the descending speed of the stretching rod 2. Adjust the position of the magnetic pole switch 3. Adjust the position of the stretching rod 4. Improve the quality of the embryo tube 5. Improve the heating conditions, or check whether there is any problem with the rotation of the preform.

reason:

1. The position of the stretching rod is not in the center of the preform  2. The blowing holes are asymmetrical and have different hole diameters. 3. The stretching ratio is too low or the blowing ratio is too small. 4. The embryo tube does not rotate in the heating furnace. 5. The embryonic tube wall thickness is not good. Injection density is uniform or uneven

Elimination method:

1. Adjust the position of the stretching rod 2. Adjust the position and diameter of the blowing hole 3. Increase the stretching or inflation ratio 4. Check the rotating device 5. Improve the quality of the preform.

reason:

1. The temperature of the upper part is too low 2. The vent hole of the mold is too far from the upper part 3. The stretching ratio is too low 4. The inflation ratio of the upper part of the bottle is too low 5. The stretching rod speed is too slow

Elimination method:

1. Heating the upper part 2. Adjust the position of the exhaust hole 3. Increase the stretching ratio 4. Change the bottle shape 5. Adjust stretch rod speed.

reason:
1. The upper part of the material does not stretch downward. 2. The bottom of the preform is designed to be thin. 3. The bottom temperature is too high.

Elimination method:

1. Delay the start of blowing time 2. Reduce the bottom temperature 3. Increase the thickness of the bottom of the preform.

reason:

1. Insufficient mold clamping pressure 2. Sealing time too early 3. Mold problem 4. The size of the preform mouth does not match the mold

Elimination method:

1. Increase the clamping pressure and adjust the angle of the clamping stay (<5 degrees). 2. Move the clamping stroke switch position backward. 3. Repair the mold or check the assembly position of the mold, such as whether the guide rails are aligned and the columns are loose or whether the mold is not properly aligned. Pressure 4. Repair the matching position of the mold teeth.

reason:

1. The delayed air blowing time is too short 2. The delayed mold opening time is too short 3. The temperature is too high 4. The exhaust valve does not work

Elimination method:

1. Extend the delayed air blowing time or increase the descending speed of the stretch rod 2. Extend the delayed mold opening time 3. Cool down 4. Clean the exhaust valve with gasoline.

PET bottle transparency is not good?

Reason:

1. The heating temperature is too high. 2. The heating time is too long. 3. Compressed air contains moisture. 4. The embryonic tube itself is opaque. 5. The embryo tube design is inappropriate. 6. The inflation rate is too small
Elimination method:

1. Lower the temperature 2. Shorten the heating time 3. Use a dryer to remove moisture 4. Improve the quality of the embryo tube, select materials, and increase the dryness of the raw materials 5. Improve the size design of the embryo tube 6. Reduce the diameter of the preform.

PET bottle whitish?

Reason:

1. The heating temperature is too low. 2. The embryonic tube wall thickness is uneven. 3. The thickness of the embryo tube is too thick and the heating penetration is insufficient.

Elimination method:

1. Increase the temperature or slow down the rotation speed 2. Improve the quality of the embryo tube 3. Reduce the thickness of the embryo tube, or try to add a heating device cover to increase the temperature distribution surface of the preform.

The position of the nozzle at the bottom of the PET bottle is offset?

Reason:

1. The blowing time is too early 2. The stretching rod has not been lowered to the bottom 3. The stretching rod deviates from the center line of the bottle axis 4. The wall thickness of the embryo tube is uneven or the injection density is uneven 5. Uneven heating

Elimination method:

1. Delay the blowing time or increase the descending speed of the stretching rod 2. Adjust the position of the magnetic pole switch 3. Adjust the position of the stretching rod 4. Improve the quality of the embryo tube 5. Improve the heating conditions, or check whether there is any problem with the rotation of the preform.

Uneven wall thickness of PET bottle?

Reason:

1. The position of the stretching rod is not in the center of the preform  2. The blowing holes are asymmetrical and have different hole diameters. 3. The stretching ratio is too low or the blowing ratio is too small. 4. The embryo tube does not rotate in the heating furnace. 5. The embryonic tube wall thickness is not good. Injection density is uniform or uneven

Elimination method:

1. Adjust the position of the stretching rod 2. Adjust the position and diameter of the blowing hole 3. Increase the stretching or inflation ratio 4. Check the rotating device 5. Improve the quality of the preform.

The upper part of the PET bottle is too thick?

Reason:

1. The temperature of the upper part is too low 2. The vent hole of the mold is too far from the upper part 3. The stretching ratio is too low 4. The inflation ratio of the upper part of the bottle is too low 5. The stretching rod speed is too slow

Elimination method:

1. Heating the upper part 2. Adjust the position of the exhaust hole 3. Increase the stretching ratio 4. Change the bottle shape 5. Adjust stretch rod speed.

The bottom of the PET preform is whitish?

Reason
1. Insufficient temperature of hot runner
2. Insufficient material temperature
Elimination method:
1. Strengthen heat insulation measures 2 . Increase the temperature of the nozzle here 3 . Properly increase the material temperature 4. Speed up the injection speed5. Reduce the holding pressure6. slow down cooling water flow.

Uneven PET preforms?

Reason:
1. Poor mold manufacturing
2. Gate hole deviation
3. Injection pressure too high
4. core shift
Elimination method:
1. Correction mold
2. Raise material temperature
3. turn down the pressure
4. Mold with high strength, high precision and adjustable core structure

PET preform gate with wire drawing?

Reason:
1. Poor insulation
2. Insufficient cooling
3. pressure in heat flow
4. Bad screw check
5. Holding pressure too low
Elimination method:
1. Guaranteed heat insulation at the gate
2. increase cooling
3. Reinforce the inverted cable
4. Clean the screw nozzle
5. increase pressure

Bending of PET preform after demoulding?

Reason:
1. Gate hole eccentric
2. uneven cooling
Elimination method:
1. Correct mold 2. Reduce the holding pressure
3. Increase injection speed 4. extended cooling
5. Clean up waterways 6. Increase cooling water pressure

Depression on the PET preform surface?

Reason:
1. Material temperature is too high
2. injection rate is too short
3. Dwell too short
4. Injection time is too short
5. Insufficient cooling
Elimination method:
1. Lower material temperature
2. Reduce the injection rate
3. increase pressure
4. increase injection time
5. increase water pressure

Private Lessons

In-Studio and Virtual Private Lessons are the best way to improve your dancing skills in the shortest period of time. Work at your own pace and receive personalized attention from our dedicated instructors.

Subscribe to our Youtube channel for more videos

Our Team

The second generation boss of the factory, has been deeply involved in the PET packaging machinery industry for 16 years, focusing on innovation and quality improvement.

Overseas manager, focusing on overseas order management, meticulous and thoughtful, ensuring that customer needs are accurate.

Chief designer, professional bottle design expert, experienced, focusing on the perfect combination of practicality and beauty.

Installation engineer, has completed 120+ project installations, is serious and responsible, and ensures stable and efficient operation of the equipment.

The second generation boss of the factory, has been deeply involved in the PET packaging machinery industry for 16 years, focusing on innovation and quality improvement.

Overseas manager, focusing on overseas order management, meticulous and thoughtful, ensuring that customer needs are accurate.

Chief designer, professional bottle design expert, experienced, focusing on the perfect combination of practicality and beauty.

Chief designer, professional bottle design expert, experienced, focusing on the perfect combination of practicality and beauty.

Chief designer, professional bottle design expert, experienced, focusing on the perfect combination of practicality and beauty.

Students Shout Out

Studio Rental

Lorem ipsum dolor sit amet, consectetur adipisicing elit, sed do eiusmod tempor incididunt ut labore et dolore magna aliqua ut enim ad minim veniam.

Studio A

Studio Size: 42ft x 21ft
Amenities: Air Conditioning, Wi-Fi, Sound System, Dressing Room, Kitchen, Toilets

Studio B

Studio Size: 68ft x 37ft
Amenities: Air Conditioning, Wi-Fi, Sound System, Dressing Room, Kitchen, Toilets

Free Trial Classes

Not sure if we are a good match for you or which style you want to learn? Free trial classes are available, one free class for each style. For more information, get in touch.
error: Content is protected !!

Get customized service for free